Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ B720 Polycarbonate/PBT Alloy Description: Naxel™ B720 is a Polycarbonate/PBT alloy. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Edgetek® XT X XT 1000 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Izod Impact, Notched | 9.59 J/cm | 18.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7691 PC UV stabilized clear polycarbonate formula for internal uses only. |
|||
Izod Impact, Notched | 9.60 - 9.60 J/cm | 18.0 - 18.0 ft-lb/in | Average value: 9.60 J/cm Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, Dry As Molded
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistan.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Kleerdex Kydex® IM62 Acrylic/PVC injection Molding Compound
(discontinued **) High impact injection molding compoundApplications: Appliances, office equipment, electrical products, tools, medical equipment, computer equipmentFeatures: IM62 has a Notched Izod impact resistance.. |
|||
Izod Impact, Notched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® TPX-HTN-000CA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256; Double 15° Notch at 73°F |
Westlake Plastics Lennite® Ultra High Molecular Weight Polyethylene Lennite UHMW-PE is a low friction engineering plastic with excellent chemical resistant and abrasive wear resistance. It is widely used in conveyors, packaging machinery, and food processing machin.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.20 mm |
18.0 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 3103 Polycarbonate Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Baye.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Makrolon® 3258 Polycarbonate, General Purpose, Mold Release, Biocompatibility It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
Izod Impact, Notched | 9.60 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers NYLON 6615 HS Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Adell BD-10 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical strength a.. |
|||
Izod Impact, Notched | 9.60 J/cm | 18.0 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl.. |