Polymer Property : Tensile Strength, Ultimate = 72.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Plaskolite Optix® CA-86 Clear General Purpose Acrylic Resin
General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin
General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D3574E
Mearthane Durethaneâ„¢ F DF-255A Closed Cell Foam Polyurethane
TDI backbone: ester.Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient of friction, abrasio..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Techmer ES Plaslube® J-50/10/TF/10 Polycarbonate, 10% GFR, 10% PTFE
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM Data
Styron CALIBREâ„¢ 200 4 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM Data
Styron CALIBREâ„¢ 200 6 Polycarbonate, General Purpose
CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins ..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Styron CALIBREâ„¢ 201-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM Data
Styron CALIBREâ„¢ 300 4 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM Data
Styron CALIBREâ„¢ 300 6 Polycarbonate, General Purpose
CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Styron CALIBREâ„¢ 301-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 72.4 MPa
10500 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4310-6 Polycarbonate
EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4510-6 Polycarbonate
EMERGEâ„¢ PC 4510-6 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Informa..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4530-6 Polycarbonate
EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 2060-6 Polycarbonate
CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
50 mm/min; ASTM D638
Styron CALIBREâ„¢ 2061-6 Polycarbonate
CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and ..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Styron CALIBREâ„¢ 302-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Styron CALIBREâ„¢ 303-06 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Tensile Strength, Ultimate 72.4 MPa
10500 psi
0.125 in, injection molded, unannealed; ASTM D638
Styron EMERGEâ„¢ 4330-6 Polycarbonate
EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information ..
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.
Tensile Strength, Ultimate 72.4 MPa
10500 psi
ASTM D638
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced
Data provided by Adell Plastics, Inc.