Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 160 - 177 °C | 320 - 351 °F | |
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Rear Barrel Temperature | 160 - 188 °C | 320 - 370 °F | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Rear Barrel Temperature | 160 - 182 °C | 320 - 360 °F | |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |
|||
Rear Barrel Temperature | 160 - 179 °C | 320 - 355 °F | |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Start Point: 170°C |
Kingfa HF-606 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowModerate UV stabilityHigh stiffnessApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co.,.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Start Point: 170°C |
Kingfa HF-618 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Start Point: 170°C |
Kingfa HF-626 Flame Retardant ABS Features:UL 94 V-0 @ 1.6-3.0mm, 5VB @ 2.0mmHigh flowHigh impact resistanceApplications:Injection moldingMonitor cabinetCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | |
LG Chemical LUCEL FW-7005 Friction and Wear Resistant POM, Oil filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
LG Chemical LUCEL FW715CS Modified POM, Friction Resistance, Abrasion Resistance Feature: Injection Molding, Modified POM, Friction Resistance, Abrasion ResistanceApplication: Gears, Printer Roller Pumps, Gear Worm WheelsCAS No. 66455-31-0 and 471-34-1Information provided by LG .. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | |
LG Chemical LUCEL N115 POM, Unreinforced, High Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | |
LG Chemical Lucet® N127 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | |
Huntsman AVALON® 65 ABX Thermoplastic Polyurethane Introduction: AVALON 65 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 65 ABX is part of the AVALON Perform Range and offers a specially designed,.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Injection Molding |
Stellarchem AB760LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Extrusion |
Stellarchem AB-860LG TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 160 - 190 °C | 320 - 374 °F | Injection Molding |
Stellarchem SV-B65E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Rear Barrel Temperature | 160 - 190 °C | 320 - 374 °F | Injection Molding |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Rear Barrel Temperature | 160 - 190 °C | 320 - 374 °F | Injection Molding |
Stellarchem SV-B75E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Rear Barrel Temperature | 160 - 177 °C | 320 - 350 °F | |
Teknor Apex Flexalloy® 9100-35 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Rear Barrel Temperature | 160 - 180 °C | 320 - 356 °F | Extrusion |
Stellarchem MP-860Q TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |