Polymer Property : Middle Barrel Temperature = 155 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Multibase TPSiV® 4000-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Middle Barrel Temperature 155 - 175 °C
311 - 347 °F
Huntsman AVALON® 60 ABX Thermoplastic Polyurethane
Introduction: AVALON 60 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 60 ABX is part of the AVALON Perform Range and offers a specially designed,..
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
Stellarchem SV-B40D TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
Stellarchem SV-B65E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
Stellarchem SV-B70E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
Stellarchem SV-B75E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
Stellarchem SV-B80E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
Middle Barrel Temperature 155 - 165 °C
311 - 329 °F
Transition, Extrusion
Stellarchem SV-B87E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..