Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D638
Flexural Yield Strength 57.2 MPa
8300 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Unnotched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
1.60 J/cm

@Temperature -40.0 °C
3.00 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Falling Dart Impact 24.85 J
18.33 ft-lb
73°F; ASTM D3029
13.6 J

@Temperature -40.0 °C
10.0 ft-lb

@Temperature -40.0 °F
ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648