Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 13.6 J | 10.0 ft-lb | 73°F; ASTM D3029 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 13.6 J | 10.0 ft-lb | 73°F; ASTM D3029 |
Spartech Crylex High Impact Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 13.6 J @Temperature -40.0 °C |
10.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetKorad is a registered trademark of Polymer Extruded Products, Inc..Information provided by Spartech. |
|||
Falling Dart Impact | 13.6 J @Temperature -40.0 °C |
10.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech Noryl® SP-5210 Specialty Sheet Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Falling Dart Impact | 13.6 J @Temperature -40.0 °C |
10.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech SP-9013 FR/ABS Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 13.6 J @Temperature -40.0 °C |
10.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech SP-9050 Low Gloss ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 13.6 J | 10.0 ft-lb | ASTM D3029 |
Total PSI 825EX Polystyrene Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of t.. |
|||
Falling Dart Impact | 13.6 J | 10.0 ft-lb | ASTM D3029 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |