Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Total 620 Polystyrene
(discontinued **) Polystyrene 620 is an impact polystyrene designed for high gloss cap layers. The polymer has been specifically designed for co extrusion processing to produce a ductile sheet with an extremely high .. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Polymer Resources ABS-GP-HH General Purpose ABS, High Heat General Purpose Acrylonitrile Butadiene Styrene, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech 617 Static Dissipative Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech Noryl® SP-5210 Specialty Sheet Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D882 |
Spartech PETG 3D Lenticular 3-D Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech SP-9080 High Heat ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | 50 mm/min; ASTM D638 |
Dow CALIBRE™ MEGARAD™ 2081-15 Polycarbonate CALIBRE™ MEGARAD™ 2081-15 resin is specially formulated to meet the radiation sterilization needs of the healthcare industry, while providing exceptional clarity, heat resistance, impact strength.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Ensinger DELRIN® AF DE588 Acetal Homopolymer, 20% PTFE filled (POM) DELRIN® AF DE588 is a 20% PTFE filled homopolymer acetal that is fully tested and certified for use by the United States Navy. The resin is manufactured by DuPont and is used extensively in a varie.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D882 |
Spartech APET SP4110 Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D638 |
Spartech Spectar® UV Copolyester Sheet Description: Copolyester SheetSpectar is a registered trademark of Eastman Chemical Company.Information provided by Spartech. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | TM R050-36 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Tensile Modulus | 2.21 GPa | 320 ksi | ASTM D-638 |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |