Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
|
RedEye On Demand PC/ABS for FDM Rapid Prototyping This thermoplastic polymer blend combines PC (Polycarbonate) and ABS (Acrylonitrile Butadiene Styrene) to produce an industrial material with a lot to offer. It combines the strength of PC with the .. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Noryl® SP-5210 Specialty Sheet Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Stratasys® PC-ABS PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior mechanical properties and heat resis.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
41.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron Pulse® 2000 ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature -40.0 - 82.2 °C |
41.0 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded Compression molded Absylux ABS is a low cost engineering plastic ideal for prototyping. It has excellent dimensional stability and lends itself to all forms of fabricationInformation provided by We.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall HHP-190 Rigid PVC, Extrusion Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall HHW-191 Rigid PVC, Extrusion Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic.. |
|||
CTE, linear | 73.8 µm/m-°C @Temperature 20.0 °C |
41.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled Information provided by Asahi Thermofil |
|||
CTE, linear | 73.8 µm/m-°C @Temperature -30.0 - 30.0 °C |
41.0 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |