Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 73.8 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
RedEye On Demand PC/ABS for FDM Rapid Prototyping
This thermoplastic polymer blend combines PC (Polycarbonate) and ABS (Acrylonitrile Butadiene Styrene) to produce an industrial material with a lot to offer. It combines the strength of PC with the ..
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech Noryl® SP-5210 Specialty Sheet
Description: Specialty SheetNoryl is a registered trademark of General Electric Company.Information provided by Spartech.
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Stratasys® PC-ABS
PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior mechanical properties and heat resis..
CTE, linear 73.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
41.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron Pulse® 2000 ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 73.8 µm/m-°C

@Temperature -40.0 - 82.2 °C
41.0 µin/in-°F

@Temperature -40.0 - 180 °F
ASTM D696
Styron Pulse® 2100LG ABS + PC
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene
Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required..
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Westlake Plastics Absylux® Acrylonitrile-Butadiene-Styrene, Compression Molded
Compression molded Absylux ABS is a low cost engineering plastic ideal for prototyping. It has excellent dimensional stability and lends itself to all forms of fabricationInformation provided by We..
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant
Absylux ABS is a low cost engineering plastic that is easy to machine and fabricate. It is an ideal material for structural applications when impact resistance, strength, and stiffness are required..
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall HHP-190 Rigid PVC, Extrusion
Georgia Gulf HHP-190 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Heat Resistance & Thermal StabilityImpact Strength & ToughnessDimensi..
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall HHW-191 Rigid PVC, Extrusion
Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic..
CTE, linear 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermylene® F6-10FG-0100 10% Glass Fiber Reinforced, Chemically Coupled
Information provided by Asahi Thermofil
CTE, linear 73.8 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Styron INSPIRE™ TF3800 Polypropylene
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010
Copyright © lookpolymers.com All Rights Reserved