Material Notes:
Description: Sign Grade SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D785
Tensile Strength, Yield 37.9 MPa
5500 psi
ASTM D638
Tensile Modulus 1.52 GPa
220 ksi
ASTM D638
Flexural Yield Strength 71.0 MPa
10300 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Unnotched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Falling Dart Impact 13.6 J
10.0 ft-lb
73°F; ASTM D3029
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature 20.0 °C
56.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523