Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System

Category Polymer , Adhesive , Thermoset
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties: Excellent adhesive for low surface energy plastics without primer.Used in potting, painting and protective coating applications.Excellent thermal and mechanical shock resistance.Ease of use.Applications: Flexible to 130% elongation, good chemical resistance. Bonds to most plastics, rubber, polyurethane, metals, ceramic and concrete. Tough, flexible, chemically resistant, non-blush clear coating with medium gloss finish. Potting compound alternative to castable polyurethanes, particularly for electrical cable/connector/transducer termination. Excellent for electrical and electronic applications as protective encapsulate against very wide range of environmental exposures, particularly moisture and sea water. Can be applied to oily surfaces. Will cure underwater. Ambient cure 24 hours or 3 hours at 100°C for full cure.
Physical Properties Metric English Comments
Oil Absorption <= 1.0 %
<= 1.0 %
60 days ambient, Isopar M
Water Absorption <= 1.0 %
<= 1.0 %
90 days ambient DI water
Viscosity 1500 cP
1500 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 9.804 MPa
1422 psi
Post Cure 180°F, 24h
Tensile Strength, Ultimate 9.915 MPa
1438 psi
Peak; Post Cure 180°F, 24h
Tensile Strength, Yield 9.915 MPa
1438 psi
Post Cure 180°F, 24h
Elongation at Break 130 %
130 %
Post Cure 180°F, 24h
Elongation at Yield 130 %
130 %
Post Cure 180°F, 24h
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
350 °F
Minimum Service Temperature, Air -45.6 °C
-50.0 °F
Processing Properties Metric English Comments
Cure Time 240 min
4.00 hour
Ambient Set
720 min
12.0 hour
Ambient, tack free
1440 min
24.0 hour
Ambient, 97% cure
240 min

@Temperature 65.6 °C
4.00 hour

@Temperature 150 °F
98% cure
Pot Life 30 - 40 min
30 - 40 min
Ambient
Descriptive Properties Value Comments
Chemical & Moisture Resistance 2
0=Lowest, 4=Highest
Color Clear with haze/slight amber
Flexibility Ranking 4.5
0=Rigid, 5=Highly Flexible