Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 76.6 °C | 170 °F | Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L4536 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.9 °C | 170 °F | ASTM D648 |
Novatec Novaloy® 9000 PVC + ABS Novaloy® 9000 is a specialty engineering alloy of ABS/PVC designed for injection molding, profile and sheet extrusion. Novaloy® 9000 has been formulated to provide excellent processing characte.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | unannealed; injection molded; ASTM D648 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Polymer Resources PPX-SF2 Modified PPO, Structural Foam Grade, Standard Flow
(Unverified Data**) Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Polymer Resources PC/TP-GP3 PC/Polyester Alloy High Impact, Superior Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 - 130 °C | 170 - 266 °F | Average value: 98.1 °C Grade Count:122 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C @Thickness 3.17 mm |
170 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
M. Holland Company AB308LG ABS Acrylonitrile Butadiene Styrene High flowGood impact resistanceHigh stiffnessApplications: Household goodsPackagingInformation provided by M. Holland |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed (0.250"); ASTM D648 |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Spartech Acrylloy 10 Acrylic Sheet Description: Acrylic SheetInformation provided by Spartech. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 E2 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L N YL038MB Availability: North AmericaForms: PelletsAdditive: Lubricant, UV Stabilizer and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Good UV Resistance and NucleatedAppeara.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 L UV (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PA6 LE BK (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and Nucleating AgentFeatures: Lubricated, Fast Molding Cycle, Good Processability, Low Extractables and NucleatedAppearance: BlackTPCI# 7.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PA6 TL10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (10%)Features: Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | Unannealed; 103°C (217°F) annealed; ASTM Data |
Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Ensinger Hydex™ 301 Rigid Polyurethane (PU) Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
Clariant Renol 6601L Nylon 66, Lubricated Data provided by Clariant Masterbatches |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | ASTM D648 |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 76.7 - 202 °C | 170 - 395 °F | Average value: 139 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Aramid Fiber Filled". Each property range of values reported is minimu.. |