Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/18T 2S Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
M. Holland Company GS411 Polystyrene
(discontinued **) Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ AT-15GP/5T Acetal-Copolymer, PTFE Lubricated
(discontinued **) Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Tensile Strength, Yield | 37.9 - 53.4 MPa | 5500 - 7750 psi | Average value: 45.0 MPa Grade Count:41 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
M. Holland Company PP200 Polypropylene Homopolymer High ESCRGood heat aging resistanceHomopolymerGood stiffnessApplications: AutomotiveHospital goodsHousehold goodsTable products |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
M. Holland Company PP410 Polypropylene Homopolymer AntistaticMedium flowGeneral purposeHomopolymerNucleatedApplications: Food containersGeneral purposeHousehold goodsToys |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Global ABS-405 FR High Impact, Flame Retardant ABS Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 37.9 MPa @Temperature 23.0 °C |
5500 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H20Z-00 Polypropylene Homopolymer This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Appl.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Spartech Crylex High Impact Acrylic Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Spartech SP-9070 ABS/PVC Flame Retardant Sheet Description: Flame Retardant SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Spartech Sta-Tuf High Impact Thermoplastic Alloy Sign Grade Sheet Description: Sign Grade SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM Data |
Styron Magnum™ 9035 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM Data |
Styron Magnum™ 347EZ ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D412 |
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an in.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 3717 Talc Filled Homopolymer Polypropylene (39.6% Mineral Content) DescriptionPolyfort® FPP 3717 is a 40% talc filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® 5142K Extrusion - Sheet - Thermoforming Polypropylene HomopolymerApplications: Extrusion, Sheet and Thermoforming ApplicationsFormolene 5142K is a high viscosity homopolymer designed primarily for thermoformed cups and container applications. It contai.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA S750 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-638 |
Bapolene® 4072NA Polypropylene Bapolene 4072NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat. Material meets the requirements of US FDA 21 CFR1777.1520.Applic.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Asahi Kasei Thermylene® P-05FG-0870 5% Glass Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D-638 |
Bapolene® 4082NA Polypropylene Bapolene 4082NA is a homopolymer polypropylene designed for fast-cycle molding applications. It is nucleated and contains antistat. Material meets the requirements of US FDA 21 CFR1777.1520.Applic.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM 638 |
PlastxWorld CEVIAN® SER23 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Tensile Strength, Yield | 37.9 MPa | 5500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |