Material Notes:
Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefits: This product offers excellent flame retardancy properties (UL 94, GWIT) combined with excellent processing, mechanical and electrical performance. Available in: Asia Pacific, Europe, Latin America and North AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: This product is ideally suited for appliance and industrial control applications such as switches, timers and contactors.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ISO 527 Type 1A
Elongation at Break 3.5 %
3.5 %
ISO 527 Type 1A
Tensile Modulus 7.00 GPa
1020 ksi
ISO 527 Type 1A
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 7.00 GPa
1020 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Dielectric Constant 3.6
3.6
IEC 60250
Dielectric Strength 40.0 kV/mm
1020 kV/in
IEC 60243
Dissipation Factor 0.050
0.050
IEC 60250
Comparative Tracking Index 500 V
500 V
Solution B; IEC 60112
600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: