Material Notes:
Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: General Purpose; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Sterilizability; High Flow; High Strength; Low Moisture Absorption; Outstanding Surface Finish; Ultra High StiffnessUses: Appliances; Automotive Applications; Automotive Interior Parts; Cell Phones; Electrical Parts; Furniture; High Gloss Applications; Hospital Goods; Medical Devices; Sporting Goods; Surgical InstrumentsInjection Molding Notes: Ixef® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Ixef® resins be dried prior to molding.Automotive Specifications ASTM D6779 PA111G50; BMW GS 93016; BOSCH N28 BN05-OX1 Color: 0008 Natural; BOSCH N28 BN05-OX1 Color: 9008 Black; GM GM7001M PAMXD6(A4,A22,A64,BA651,G30,MS1700,NS335) Color: 9008 Black; GM GM7001M PAMXD6(A4,A22,A64,BA751,G30,MS1700,NS350) Color: NT NaturalInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.64 g/cc
0.0592 lb/in³
Dry; ISO 1183
Filler Content 50 %
50 %
Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength at Break 260 MPa
37700 psi
ISO 527-2
Elongation at Break 2.2 %
2.2 %
ISO 527-2
Tensile Modulus 20.0 GPa
2900 ksi
ISO 527-2
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Melt Temperature 280 °C
536 °F
Mold Temperature 120 - 140 °C
248 - 284 °F
Drying Temperature 120 °C
<br>@Time 1800 - 5400 sec
248 °F
<br>@Time 0.500 - 1.50 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Black; Colors; Natural
Form Pellets
Injection Rate Fast
Processing Technique Injection Molding
RoHS Compliance RoHS Compliant
UL File Number E95746 (Global)