Ashley Polymers Ashlene® 67MG Nylon 66, Glass/Mineral reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 67MG Nylon 66, Glass/Mineral reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A glass/mineral reinforced Nylon 66 designed for high strength and dimensional stability.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131 MPa
19000 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648
Users viewing this material also viewed the following: