Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 4 = 302 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst CAT 10 Polyolefin
Catalyst CAT 10 is a high density based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin
Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst LV/1 Polyolefin
Catalyst LV/1 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst LV/1LR Polyolefin
Catalyst LV/1LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or ..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin
Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2 Polyolefin
Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam ..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin
Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2LR Polyolefin
Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or ..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin
Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/4 Polyolefin
Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st..
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Cogegum® GFR/350 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes...
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE)
POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-HF Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-HF is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 4 150 - 170 °C
302 - 338 °F
Solvay Specialty Polymers Polidiemme® G/220 Thermoset Elastomer (TSE)
Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (S..
Zone 4 150 °C
302 °F
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable
Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDP..
Copyright © lookpolymers.com All Rights Reserved