Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 150 °C | 302 °F | |
Termopol Termoton® K2GA5050A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 150 °C | 302 °F | |
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 150 - 180 °C | 302 - 356 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Zone 1 | 150 - 160 °C | 302 - 320 °F | |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |
|||
Zone 1 | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon. |
|||
Zone 1 | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Kolon ELLAS K-787A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 150 - 160 °C | 302 - 320 °F | |
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ.. |
|||
Zone 1 | 150 - 160 °C | 302 - 320 °F | |
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera.. |
|||
Zone 1 | 150 - 160 °C | 302 - 320 °F | |
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst LV/1 Polyolefin Catalyst LV/1 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Polyolefin Catalyst PS/2 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that take place by exposure of the pipe to water or steam .. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LR Polyolefin Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or .. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/4 Polyolefin Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes... |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® S/I 20 Polyethylene, Crosslinked (XLPE) POLIDAN® S/I 20 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for injection molding.Features: Crossl.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 1 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 1 | 150 °C | 302 °F | |
Borealis Borcell™ HE1123 High Density Polyethylene Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by.. |
|||
Zone 1 | 150 °C | 302 °F | |
Borealis Visico™/Ambicat™ LE4421/LE4472 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4472 is a silane crosslinkable black compound designed for covering/insulation of overhead cables. The base material Visico™ LE4421 in combination with the catalyst m.. |
|||
Zone 1 | 150 °C | 302 °F | |
Borealis Visico™/Visico™ ME4425/LE4438 Polyethylene Visico™ ME4425 / Visico™ LE4438 is a silane crosslinkable natural compound designed for low voltage power cables up to 6 kV. Visico™ ME4425 and Visico™ LE4438 is a combination of a Visico™ bas.. |
|||
Zone 1 | 150 °C | 302 °F | |
Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE442.. |
|||
Zone 1 | 150 °C | 302 °F | |
Borealis Visico™/Ambicat™ LE4421/LE4476 Polyethylene Compound, Crosslinkable Visico™ LE4421 / Ambicat™ LE4476 is a silane crosslinkable natural compound designed for low voltage power cables up to 6kV. The base material Visico™ LE4421 in combination with the catalyst mas.. |