Polymer Property : Zone 4 = 200 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® M270UV POM, UV Resistant  (Unverified Data**)
Celcon® M270UV is an acetal copolymer developed as a natural UV light stabilized lower molecular weight, high-flow grade designed for superior moldability in multi-cavity or hard to fill injection ..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® AM90S POM, Specialty  (Unverified Data**)
Hostaform® acetal copolymer grade AM90S is a standard melt flow acetal copolymer grade containing an antimicrobial ingredient. Hostaform® AM90S provides the same physical and mechanical performan..
Zone 4 180 - 200 °C
356 - 392 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical
Zone 4 185 - 200 °C
365 - 392 °F
Extrusion Molding
Kolon ELLAS K-490AB Ester Based Thermoplastic Polyurethane
ApplicationsExtrusionInjectionFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Zone 4 185 - 200 °C
365 - 392 °F
Extrusion Molding
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane
ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon.
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Catalyst PS/4 Polyolefin
Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st..
Zone 4 150 - 200 °C
302 - 392 °F
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
Zone 4 190 - 200 °C
374 - 392 °F
Injection
Lubrizol ESTANE® GP80AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 80AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® AM90S POM, Specialty
Hostaform« acetal copolymer grade AM90S is a standard melt flow acetal copolymer grade containing an antimicrobial ingredient. Hostaform« AM90S provides the same physical and mechanical performan..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® C 9021 XAP2 LS POM, UV Resistant
POM copolymerInformation provided by Celanese
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® S 27242 XAP² ™ POM, Impact Modified
Easy flow, impact modified injection molding grade, with good low temperature impact strength and good weld line strength and reduced emissions. Emission according to VDA 275 < 5 mg/kgInformation pr..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9362 POM, Impact Modified
Hostaform« acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform« S 9362 provides good impact strength while improving modulus and weld ..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® S 27242 XAP2 ™ POM, Impact Modified
Easy flow, impact modified injection molding grade, with good low temperature impact strength and good weld line strength and reduced emissions. Emission according to VDA 275 < 5 mg/kgInformation pr..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified
POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® GC10 POM, 10% Glass Reinforced
Celcon« GC10 acetal copolymer is a 10% glass reinforced acetal for improved strength and stiffness.Information provided by Celanese
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® M140 POM, Unfilled
Celcon« acetal copolymer grade M140 is a moderately high flow general purpose injection molding grade. It is designed for use in applications requiring some enhanced flow characteristics over the s..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® M270™ POM, Unfilled
Celcon« acetal copolymer grade M270Ö is a lower molecular weight, high - flow grade designed for superior moldability in multi-cavity, intricate or hard to fill molds applications.Information prov..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® M450 POM, Unfilled
Celcon« acetal copolymer grade M450 is an extremely low viscosity grade for optimal cycle performance in very thin walls or long, narrow flow paths in injection molding.Information provided by Cela..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® M90™ POM, Unfilled
Celcon acetal copolymer grade M90Ö is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film. This gr..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Celcon® MR90B POM, Specialty
Celcon« MR90B is a standard flow specialty media resistant grade developed for improved bleach resistance.Information provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9363 POM, Impact Modified
Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® SXT90Z-02 XAP POM, Impact Modified
Hostaform« acetal copolymer grade SXT90Z-02 XAP is UV stabilized, impact modified material available in a range of colors for automotive interior applications plus meets the typical low emission re..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® S 27064 XAP2® POM, Impact Modified
Description: Easy flowing, elastomer-containing injection molding type based on HOSTAFORM C 27021 with high toughness and reduced emissionsHB. Burning rate ISO 3795 and FMVSS 302 < 100 mm/min for mo..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® MC270-HM POM, Mineral Reinforced  (Unverified Data**)
Celcon® MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® MC90 POM, Mineral Reinforced  (Unverified Data**)
Celcon® acetal copolymer grade MC90 is a mineral reinforced grade offering low warp, improved dimensional stability, improved stiffness, improved practical impact and retention of other base resin ..
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Celcon® MR270B POM, Specialty  (Unverified Data**)
Celcon® MR270B is a high flow specialty media resistant grade developed for improved bleach resistance.Improved media resistance to bleach with higher flowStandard reciprocating screw injection mol..
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Hostaform® S 9243 XAP² ™ LS POM, Impact Modified  (Unverified Data**)
POM copolymer, modifiedImpact modified, UV stabilizedInformation provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetImpact modified, improved modulus and weld line, low emissionInformation provided by Celanese
Zone 4 180 - 200 °C
356 - 392 °F
Celanese Hostaform® XT 90 POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetHighly impact modified, improved weld lineInformation provided by Celanese
Zone 4 190 - 200 °C
374 - 392 °F
Celanese Celcon® MC90-HM POM, Mineral Reinforced
Celcon« MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).Information provided by Celanese