Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® LW90 POM, Tribological
(Unverified Data**) Celcon® LW90 is a nominal 9 melt flow rate based material specifically formulated for high speed, low wear applications against metals. LW90 conforms to applicable FDA regulations governing food co.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® MC270 POM, Mineral Reinforced
(Unverified Data**) Celcon® MC270 is a mineral coupled acetal copolymer designed for applications requiring improved stiffness, lower mold shrinkage and reduced warpage while maintaining the mechanical performance cha.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® UV270Z POM, UV Resistant
(Unverified Data**) Celcon® UV270Z is a nominal 27 melt flow rate acetal copolymer which has been specially stabilized to prevent discoloration and deterioration of mechanical properties from ultraviolet light exposur.. |
|||
Zone 4 | 185 - 200 °C | 365 - 392 °F | Extrusion Molding |
Kolon ELLAS K-429A Ester Based Thermoplastic Polyurethane ApplicationsIndustry PartsOutsole of Soccer ShoeHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 4 | 185 - 200 °C | 365 - 392 °F | Extrusion Molding |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 4 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® MC90 POM, Mineral Reinforced Celcon« acetal copolymer grade MC90 is a mineral reinforced grade offering low warp, improved dimensional stability, improved stiffness, improved practical impact and retention of other base resin .. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® XT 20 POM, Impact Modified Preliminary Data SheetInformation provided by Celanese |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M140 POM, Unfilled Celcon« acetal copolymer grade M140 is a moderately high flow general purpose injection molding grade. It is designed for use in applications requiring some enhanced flow characteristics over the s.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M90LF POM, Unfilled Hostaform« acetal copolymer grade M90LF is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film.Info.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® AM90S Plus POM, Specialty Hostaform« acetal copolymer grade AM90S Plus is a standard melt viscosity acetal copolymer material containing an antimicrobial ingredient. AM90S Plus reaches maximum efficacy more rapidly than st.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® S 9243 XAP² ™ POM, Impact Modified POM copolymer, modifiedInformation provided by Celanese |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9363 POM, Impact Modified Hostaform« acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform« S 9363 provides good impact strength while improving modulus and weld line strength o.. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9364 POM, Impact Modified Hostaform« acetal copolymer grade S 9364 is highly impact modified grade for demanding applications. Hostaform« S 9364 provides a significant improvement in impact strength and flexibility over s.. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9364 WS 10/1570 POM, UV Resistant Preliminary Data SheetInformation provided by Celanese |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® SXT90Z-02 XAP POM, Impact Modified Hostaform« acetal copolymer grade SXT90Z-02 XAP is UV stabilized, impact modified material available in a range of colors for automotive interior applications plus meets the typical low emission re.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® S 9243 XAP2 ™ POM, Impact Modified POM copolymer, modifiedIt is normally not necessary to dry HOSTAFORM. However, should there be surface moisture (condensate) on the molding compound as a result of incorrect storage, drying is requi.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® LW90-S2 POM, Tribological
(Unverified Data**) Celcon® LW90-S2 is a preblended low wear formulation of M90 base polymer containing 2% silicone. This standard low friction, low wear product performs well in many applications including those inv.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M140 POM
(Unverified Data**) Celcon® acetal copolymer grade M140 is a moderately high flow general purpose injection molding grade. It is designed for use in applications requiring some enhanced flow characteristics over the s.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® M270™ POM
(Unverified Data**) Celcon® acetal copolymer grade M270™ is a lower molecular weight, high - flow grade designed for superior moldability in multi-cavity, intricate or hard to fill molds applications.General purpose,.. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Celcon® M90-45H POM, UV Resistant
(Unverified Data**) Celcon® M90-45H is an acetal copolymer which has been stabilized to give protection against property and color degradation in interior applications where UV exposure is anticipated.Formulated in cu.. |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® WR90Z POM, UV Resistant
(Unverified Data**) Celcon® WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of .. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® C 27021 XAP² ™ LS colored POM, UV Resistant
(Unverified Data**) PolyacetalcopolymerLow Emission UV stabilizedInformation provided by Celanese |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Hostaform® EC140CF10 POM, 10% Specialty
(Unverified Data**) Hostaform® acetal copolymer grade EC140CF10 is a 10% carbon fiber reinforced grade for increase strength, stiffness and electrical conductivity.10% carbon fiber, electrostatic dissipative gradeInfo.. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9363 POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9363 is an impact modified grade for demanding applications. Hostaform® S 9363 provides good impact strength while improving modulus and weld line strength o.. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® S 9363 XAP² ™ POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9363 XAP2 ™ is an impact modified grade for demanding applications. Hostaform® S 9363 XAP2 ™ provides good impact strength while improving modulus and weld.. |
|||
Zone 4 | 180 - 200 °C | 356 - 392 °F | |
Celanese Hostaform® XT 20 POM, Impact Modified
(Unverified Data**) Preliminary Data SheetHighly Impact ModifiedInformation provided by Celanese |
|||
Zone 4 | 190 - 200 °C | 374 - 392 °F | |
Celanese Celcon® LW90-F2 POM, Tribological Celcon« LW90-F2 is an acetal copolymer formulated with a nominal 9 melt flow rate base polymer and a standard level of polytetrafluoroethylene filler (PTFE). It is designed for use in wear applicat.. |