Silikony Polskie Polastosil M-56 Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Silikony Polskie
Trade Name Polastosil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silikony Polskie Polastosil M-56 Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rubber with strong hardness
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
Before Curing
Viscosity 45000 cP
45000 cP
Before Curing
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
After Curing
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
After Curing
Tensile Strength at Break 2.00 MPa
290 psi
After Curing
Elongation at Break 100 %
100 %
After Curing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Processing Properties Metric English Comments
Cure Time <= 1440 min
<= 24.0 hour
Curing
Pot Life 30 min
30 min
Curing
Descriptive Properties Value Comments
Color Red