Material Notes:
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistance property.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 1.60 g/cc
0.0578 lb/in³
Dried at 110°C
Grain Size <= 6000 µm
<= 6000 µm
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00312 GPa

@Temperature 1100 °C
0.453 ksi

@Temperature 2010 °F
0.00735 GPa

@Temperature 110 °C
1.07 ksi

@Temperature 230 °F
0.00883 GPa

@Temperature 1500 °C
1.28 ksi

@Temperature 2730 °F
Compressive Strength 7.35 MPa

@Temperature 1100 °C
1070 psi

@Temperature 2010 °F
Cold Crushing
7.35 MPa

@Temperature 800 °C
1070 psi

@Temperature 1470 °F
Cold Crushing
8.83 MPa

@Temperature 1300 °C
1280 psi

@Temperature 2370 °F
Cold Crushing
12.7 MPa

@Temperature 110 °C
1850 psi

@Temperature 230 °F
Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity 0.511 W/m-K
3.55 BTU-in/hr-ft²-°F
1.16 W/m-K
8.05 BTU-in/hr-ft²-°F
1.34 W/m-K
9.30 BTU-in/hr-ft²-°F
1.39 W/m-K
9.65 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Fe2O3 1.5 %
1.5 %
Descriptive Properties Value Comments
Permanent Linear Change <-0.05%
800°C
<-0.08%
1100°C
<-0.2%
1500°C
-0.9 - 0.9%
1300°C
Refractoriness <1900°C
Copyright © lookpolymers.com All Rights Reserved