Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.39 W/m-K | 9.65 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.39 W/m-K | 9.65 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.39 W/m-K | 9.65 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |