Physical Properties | Metric | English | Comments |
---|---|---|---|
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST LC45 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST LC60 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST LC80 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST LC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST ULCC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 11 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 15 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 4 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 7 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 9 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFCAST LC95 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics REFINSUL 13LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Grain Size | <= 6000 µm | <= 6000 µm | |
Sharadaa Ceramics ZAP 012 Smart Cast Application Special Properties: Patching At Hot Conditions, Easy InstallationIndustry: All IndustryApplication: All type of Rotary Kilns, AL/CU Melting Furnaces, Rolling Mills, Forgoing Furnaces, IncineratorsIn.. |