Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.34 W/m-K | 9.30 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.34 W/m-K | 9.30 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.34 W/m-K | 9.30 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 7 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.34 W/m-K | 9.30 BTU-in/hr-ft²-°F | |
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |
|||
Thermal Conductivity | 1.34 W/m-K | 9.30 BTU-in/hr-ft²-°F | |
Epoxy Technology EPO-TEK® 430 Epoxy Product Description: A two component, copper-filled, electrically and thermally conductive epoxy for adhesive bonding in electronics. It may be used at the PCB level for interconnecting, grounding .. |
|||
Thermal Conductivity | 1.34 - 2.87 W/m-K @Temperature 1450 °C |
9.30 - 19.9 BTU-in/hr-ft²-°F @Temperature 2640 °F |
Varies directly with relative density (8-16%) |
ERG Aerospace Duocel® Silicon Carbide Foam Silicon Carbide (SiC) foam is a porous, open-celled structure made from an interconnected lattice of ceramic ligaments. The pattern of cells and ligaments repeats regularly throughout the entirety o.. |