Qualchem Danamid FGFL0-20 Polyamide 6, 20% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Qualchem Zrt.
Trade Name Danamid
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Qualchem Danamid FGFL0-20 Polyamide 6, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced with glass fiber. Flame retardant, with halogens (V-0)Information provided by Qualchem Zrt.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
DIN 53479
Filler Content 18 - 22 %
18 - 22 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
50 mm/min; ISO 527-1,2
Elongation at Break 3.5 %
3.5 %
ISO 527-1,2
Tensile Modulus 6.40 GPa
928 ksi
ISO 527-1,2
Charpy Impact Unnotched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
DIN 53461
Flammability, UL94 V-0

@Thickness 4.00 mm
V-0

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53482
Comparative Tracking Index 450 V
450 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
DIN 53714