Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00312 GPa @Temperature 1100 °C |
0.453 ksi @Temperature 2010 °F |
|
Sharadaa Ceramics REFINSUL 15LI Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |