Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity

Category Ceramic
Manufacturer Sharadaa Ceramics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistance property.Information provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density 1.45 g/cc
0.0524 lb/in³
Dried at 110°C
Grain Size <= 6000 µm
<= 6000 µm
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00588 GPa

@Temperature 1100 °C
0.853 ksi

@Temperature 2010 °F
0.0103 GPa

@Temperature 110 °C
1.49 ksi

@Temperature 230 °F
0.0113 GPa

@Temperature 1500 °C
1.64 ksi

@Temperature 2730 °F
Compressive Strength 2.94 MPa

@Temperature 1100 °C
427 psi

@Temperature 2010 °F
Cold Crushing
2.94 MPa

@Temperature 800 °C
427 psi

@Temperature 1470 °F
Cold Crushing
4.90 MPa

@Temperature 110 °C
711 psi

@Temperature 230 °F
Cold Crushing
4.90 MPa

@Temperature 1300 °C
711 psi

@Temperature 2370 °F
Cold Crushing
Thermal Properties Metric English Comments
Thermal Conductivity 0.372 W/m-K
2.58 BTU-in/hr-ft²-°F
1.34 W/m-K
9.30 BTU-in/hr-ft²-°F
1.39 W/m-K
9.65 BTU-in/hr-ft²-°F
1.51 W/m-K
10.5 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Fe2O3 3.5 %
3.5 %
Descriptive Properties Value Comments
Permanent Linear Change <-0.12%
1100°C
<-0.6%
1500°C
<-0.6%
800°C
-0.7 - 0.7%
1300°C
Refractoriness <1750°C