Mechanical Properties Metric English Comments
Compressive Strength 2.94 MPa

@Temperature 1100 °C
427 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 2.94 MPa

@Temperature 800 °C
427 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 11LI Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 2.94 MPa

@Temperature 1100 °C
427 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 2.94 MPa

@Temperature 800 °C
427 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 2.94 MPa

@Temperature 1300 °C
427 psi

@Temperature 2370 °F
Cold Crushing
Sharadaa Ceramics REFINSUL 8S Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..
Compressive Strength 2.94 MPa

@Temperature 800 °C
427 psi

@Temperature 1470 °F
Cold Crushing
Sharadaa Ceramics Sharada LTM 0.9 Insulating Castable
Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 2.94 - 4.90 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 711 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories DC-2BS Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 4.41 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 640 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories GUN-80L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 1000 °C,
Time 10800 sec
427 - 1140 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 500 °C,
Time 10800 sec
427 - 1140 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 1000 °C,
Time 10800 sec
427 - 1140 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-120S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 500 °C,
Time 10800 sec
427 - 1140 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 1000 °C,
Time 10800 sec
427 - 1140 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT135S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 3.92 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 569 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-50S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 3.92 MPa

@Temperature 500 °C,
Time 10800 sec
427 - 569 psi

@Temperature 932 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-50S Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PT-140 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PAC-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 2.94 - 7.85 MPa

@Temperature 110 °C,
Time 86400 sec
427 - 1140 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PT-150 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved