Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0103 GPa @Treatment Temp. 815 °C |
1.49 ksi @Treatment Temp. 1500 °F |
|
Pyrotek Pyrocast AR Castable Refractory Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro.. |
|||
Modulus of Rupture | 0.0103 GPa @Temperature 110 °C |
1.49 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFCAST A SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Modulus of Rupture | 0.0103 GPa @Temperature 110 °C |
1.49 ksi @Temperature 230 °F |
|
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan.. |