Polymer Property : Thermal Conductivity = 2.58 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.372 W/m-K
2.58 BTU-in/hr-ft²-°F
Sharadaa Ceramics REFINSUL 13 Insulating Castables Medium/High Purity
Description: We offer our clients Insulating Castables that are available in medium as well as high purity. Widely used in various industries, these are renowned for their strength and heat resistan..