Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shakespeare Isocorâ„¢ SC45BT Nylon 610

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer Shakespeare Company
Trade Name Isocor™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shakespeare Isocorâ„¢ SC45BT Nylon 610.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isocorâ„¢ SC45BT is a medium viscosity PA-610 based copolymer. This resin is specifically suited for clear applications requiring increased solvent resistance and impact properties. Isocorâ„¢ SC45BT is also used in applications requiring improved dimensional stability This resin can be processed with conventional techniques. Used for injection molding, monofilaments / bristles, and film extrusion.Information provided by Shakespeare Company.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D 792
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Tensile Strength at Break 47.6 MPa
6900 psi
ASTM D 638
Elongation at Break 51 %
51 %
ASTM D 638
Tensile Modulus 3.10 GPa
450 ksi
ASTM D 638
Izod Impact, Notched 0.481 J/cm
0.900 ft-lb/in
ASTM D 256
Gardner Impact 4.63 J

@Temperature 23.0 °C
3.42 ft-lb

@Temperature 73.4 °F
ASTM D 5420
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 70.0 °C
158 °F
ASTM D 3418