Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 47.6 MPa | 6900 psi | chs 2 in/min; ASTM D638 |
Network Polymers NPS 80-1800 Crystal Polystyrene Description: Injection Molding Grade, High Melt FlowInformation provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | |
Lucas-Milhaupt Silvabrite® 100® Lead-Free Solder Silvabrite 100® was developed to meet market demands for a safe and easy to use solder for drinking water systems and other applications. Silvabrite 100® is a lead-free and antimony-free, non-.. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | ASTM D 638 |
Shakespeare Isocorâ„¢ SC45BT Nylon 610 Isocorâ„¢ SC45BT is a medium viscosity PA-610 based copolymer. This resin is specifically suited for clear applications requiring increased solvent resistance and impact properties. Isocorâ„.. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | 94% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | 94% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | ASTM D638 |
Eastman Tenite 485E3720008 Cellulose Acetate Butyrate, Clear, Trsp Applications:Toys/Sporting goodsProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties including toughness, hardness, strength, surface gloss, clarity,.. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | ASTM D638 |
Americas Styrenics STYRON® 675 High Heat Crystal Polystyrene Product CharacteristicsHigh heatMedium flowFood Contact CompliantUL Classification 94HBTypical ApplicationsThin-walled partsInformation provided by AmericasStyrenics LLC. |
|||
Tensile Strength at Break | 47.6 MPa | 6900 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 6630 Antistatic Polystyrene Characteristics Easy flow Excellent transparency Processing Extrusion Applications For glossy cap layer on HIPS To prevent dust patterns on thermoformed products Material Status: Commercial : Acti.. |