Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID SG2460B PA66+GF46%, General purpose, Good Surface Feature: Injection Molding, PA66+GF46%, General purpose, Good SurfaceApplication: Automotive (Side Mirror Base PlateCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Porene KU650 Acrylonitrile Butadiene Styrene Applications:injection moldingautomotive parts such as instrument panels, console boxes, switches, automotive louvers, ectelectrical appliances |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® HI2303 PBT+GF30% Description: Injection Molding, PBT+GF30%, High ImpactApplication: IT/OA, E&E (Bobbin, Switch)CAS No. 9003-01-04, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® VIC4311 PBT (Asia Pacific) |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® VIC4350 PBT (Asia Pacific) |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 6.35 mm |
2.57 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® MG-0330 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 6.35 mm |
2.57 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 6.35 mm |
2.57 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® MG-0330 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.37 J/cm @Thickness 6.35 mm |
2.57 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N190HF PPE+HIPS (Asia Pacific) |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N225Z PPE+HIPS (Asia Pacific) PPE+PS 115deg,C, FR V-0 |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PPO534 PPE+HIPS (Asia Pacific) PPO/PS unfilled high heat |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Notched | 1.37 J/cm @Temperature 23.0 °C |
2.57 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H511W High Density Polyethylene Wire & Cable Grade Key Characteristics: Contains special metal deactivator, high mechanical properties, high speed extrusionRecommended Applications: Insulation of communication cablesInformation provided by SCG Che.. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Asia Pacific) PPE/PS, 80degC, FR V-0, high flow |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | |
Zylog Hipolyene® 6131 XF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | |
Zylog Hipolyene® 6251 Y M4 C Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | |
Zylog Hipolyene® 6251 Y M4 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® H12T Unreinforced High Impact PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Izod Impact, Notched | 1.37 J/cm @Temperature 23.0 °C |
2.57 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers VESPEL TP-8929 Polyimide DuPont Vespel TP-8929 parts are specified for mechanical and thermal performance. TP-8929 parts offer low friction, dimensional stability, low outgassing, radiation resistance, and creep resistance... |
|||
Izod Impact, Notched | 1.37 J/cm | 2.57 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® K130IM 30% Glass Fiber Reinforced Impact Modified PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |