Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 43.1 MPa | 6250 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L0148 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po.. |
|||
Tensile Strength, Yield | 43.1 - 103 MPa | 6260 - 15000 psi | Average value: 75.1 MPa Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Yield | 43.1 MPa | 6250 psi | ASTM D638 |
M. Holland Company AB105 ABS Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Household Goods, Packaging Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical AF312A ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
50 mm/min; ASTM D638 |
LG Chemical MP211 ABS, Low Gloss, Metal Plating Feature: Injection Molding, High Flow, Metal PlatingApplication: Decorative Parts (Home Appliance Door Handle Etc)CAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Tensile Strength, Yield | 43.1 MPa | 6250 psi | ASTM D638 |
Iran Petrochemical (PCC) SD-0150 Acrylonitrile Butadiene Styrene General Purpose ABS, SD 0150 grade, is a rigid thermoplastic with good processing characteristics. It is a high flow injection molding grade with considerable impact strength and medium heat deflec.. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® MG-0330 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0315 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0970 MS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® MG-0330 ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6260 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 43.1 MPa | 6250 psi | ASTM D638 |
Eastman Tenite 285E0V16304 Cellulose Acetate Butyrate, Clear, Trsp Applications:DisplaysProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-11G ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D638 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron SHF-50+ ABS Injection Molding Grade High Flow High Gloss, Fancy ApplicationsInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade Medium Impact, High Gloss, High FlowInformation provided by Bhansali |
|||
Tensile Strength, Yield | 43.1 MPa @Thickness 3.20 mm |
6260 psi @Thickness 0.126 in |
Type 1; ASTM D-638 |
Bhansali Engineering Abstron IM-17A(DLW) ABS Injection Molding Grade Medium Impact, Medium Flow ,White UndertoneInformation provided by Bhansali |