Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.02 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
7.53 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 4.02 J/cm @Thickness 6.35 mm |
7.53 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 4.02 J/cm | 7.53 ft-lb/in | ASTM D256 |
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic SKYGREEN is a series of aliphatic polyester and aliphatic/aromatic copolyester that is degraded into water and carbon dioxide by microorganismsSKYGREEN, biodegradable thermoplastics, has been develo.. |
|||
Izod Impact, Notched | 4.02 J/cm @Thickness 6.35 mm |
7.53 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |