Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 7.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Flexural Strength 108 MPa
15700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 5.30 GPa
768 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.785 J/cm

@Thickness 3.17 mm
1.47 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 - 6.00 mm
HB

@Thickness 0.0591 - 0.236 in
Users viewing this material also viewed the following: