Polymer Property : Tensile Strength, Yield = 12100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 83.4 MPa
12100 psi
ISO 527
Honeywell Aegis™ HFX High Barrier Nylon  (discontinued **)
Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is ..
Tensile Strength, Yield 83.4 MPa

@Thickness 3.20 mm
12100 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose
Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
Tensile Strength, Yield 83.4 MPa

@Thickness 3.20 mm
12100 psi

@Thickness 0.126 in
5mm/min; ASTM D638
LG Chemical LUMID GP3400B(W) PA66+MF40%, General Purpose
Feature: Injection Molding, PA66+MF40%, General PurposeApplication: Automotive (Engine Cover)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical
Tensile Strength, Yield 83.4 MPa

@Thickness 3.20 mm
12100 psi

@Thickness 0.126 in
50mm/min; ASTM D638
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM D638
Spartech Polycast Poly 2000 (Mil-P-25690;Class 1) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM D638
Spartech Polycast Poly 2000 (Mil-P-25690;Class 2) Cell Cast Acrylic
Description: Cell Cast AcrylicInformation provided by Spartech.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VB-4921 ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® XK-2307 PPS
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Starex® VB-4921 ABS, Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
5 mm/min; ASTM D638
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM 638
PlastxWorld CEVIAN® SERG3 30% GF ABS
Glass fiber reinforced and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM 638
PlastxWorld CEVIAN® SKG20 20% GF ABS
Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast..
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM D638
Cheng Yu Plastic N66C1 Nylon 66, 10% Mineral Reinforced
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM D638
Cheng Yu Plastic NGC3 Nylon 6, 30% Mineral Reinforced
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM D638
Cheng Yu Plastic FRCV150 Flame Retardant Nylon 66, 20% Mineral Reinforced
Tensile Strength, Yield 83.4 MPa
12100 psi
ASTM D638
Cheng Yu Plastic ML3410 PC, 10% Glass Fiber