Samsung Cheil Industries Infino® EN-1052 PC, FR

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Unreinforced, Flame Retardant
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® EN-1052 PC, FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 250 °C
18 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 58.8 MPa
8530 psi
50 mm/min; ASTM D638
Flexural Strength 83.4 MPa
12100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 5.88 J/cm

@Thickness 6.35 mm
11.0 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 6.40 mm
264 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 142 °C
288 °F
B/50; ISO R306
UL RTI, Electrical 130 °C
266 °F
UL RTI, Mechanical with Impact 130 °C
266 °F
UL RTI, Mechanical without Impact 130 °C
266 °F
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
V-0

@Thickness 1.50 - 3.00 mm
V-0

@Thickness 0.0591 - 0.118 in