ExxonMobil Mobil DTE 724 Oil

Category Fluid , Lubricant
Manufacturer ExxonMobil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil DTE 724 Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mobil DTE 724 Oil was developed for higher-output gas turbines such as the General Electric Heavy Duty Gas Turbine Frame 7000. Mobil DTE 724 Oil offers excellent thermal and oxidative stability, and resistance to deposit formation to meet the high temperature demands of gas turbines.Mobil DTE 724 Oil was developed for higher-output gas turbines such as the General Electric Heavy Duty Gas Turbine Frame 7000. Mobil DTE 724 Oil meets the performance requirements of General Electric specification GEK-32568C.
Physical Properties Metric English Comments
Specific Gravity 0.866 g/cc
0.866 g/cc
API Gravity 32.2 °
32.2 °
Viscosity Measurement 95
95
Index
Kinematic Viscosity at 40°C (104°F) 31 cSt
31 cSt
Kinematic Viscosity at 100°C (212°F) 5.4 cSt
5.4 cSt
Oxidative Stability 4000 hour
4000 hour
Turbine Oil Stability Test (TOST); ASTM D943
ASTM Color 1.5
1.5
ASTM D1500
Thermal Properties Metric English Comments
Pour Point -12.0 °C
10.4 °F
Flammability Test 241
241
Fire Point [°C]
310
310
Auto Ignition [°C]
Flash Point >= 216 °C
>= 421 °F
Component Elements Properties Metric English Comments
H2O 0.00 %
0.00 %
Zinc, Zn 0.00 %
0.00 %
Chemical Properties Metric English Comments
Total Acid Number <= 0.20
<= 0.20
ASTM D664
Descriptive Properties Value Comments
Copper Strip Corrosion 1B
3 hrs @ 100°C
Foam Sequence I, ASTM D974 20/0
Foam Sequence II, ASTM D893 50/0
Foam Sequence III, ASTM D893 20/0
Rust Prevention, Distilled Water pass
ASTM D665A
Rust Prevention, Synthetic Sea Water pass
ASTM D665B
Sediment, vol % 0.005 (max)