Axiall 3152 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 3152 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 3152 is a twin screw powder blend NSF approved for the extrusion of potable water and drain waste and vent pipe application.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
ASTM D-2240
Tensile Strength, Yield 49.0 MPa
7100 psi
ASTM D-638
Tensile Modulus 2.78 GPa
403 ksi
ASTM D-638
Flexural Strength 77.9 MPa
11300 psi
ASTM D-790
Flexural Modulus 2.58 GPa
374 ksi
ASTM D-790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 170 kJ/m²
80.8 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 199 °C
390 °F
Descriptive Properties Value Comments
Cell Classification 12454B
ASTM D-1784
Users viewing this material also viewed the following: