Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.88 J/cm | 11.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC5400 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 5.88 J/cm | 11.0 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333NW High Impact Nylon 66 Impact -resistant, dimensional safetyApplications Wheel coversInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000HZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive (Door Handle)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000LZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish)CAS No. 9003-01-04, 24968-12-5 and 103598-77-2Information provide.. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5008BF FR PC/ABS, Flame Retardance, Heat Resistance Description: Injection Molding, PC/ABS, Flame Retardance, Heat ResistanceApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SR3108FC PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
Izod Impact, Notched | >= 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 5.88 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.0 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Izod Impact, Notched | 5.88 J/cm | 11.0 ft-lb/in | ASTM D 256 |
MRC Polymers NAXELL™ PC210HR General Purpose Polycarbonate, High MFR • Black onlyInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.35 mm |
11.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® EN-1052 PC, FR Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 6.35 mm |
11.0 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® EN-1052 PC, FR Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® SC-1220R PC, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 5.88 J/cm @Thickness 3.17 mm |
11.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1015 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |