Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics ULTEM AR9300 PEI

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics ULTEM AR9300 PEI.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 4.2 g/10 min

@Load 6.60 kg,
Temperature 337 °C
4.2 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 5 mm/min; ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
5 mm/min; ASTM D638
Flexural Yield Strength 241 MPa
35000 psi
2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 9.65 GPa
1400 ksi
2.6 mm/min, 100 mm span; ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
5.34 J/cm

@Thickness 3.20 mm
10.0 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 212 °C

@Thickness 6.40 mm
414 °F

@Thickness 0.252 in
unannealed; ASTM D648
Glass Transition Temp, Tg 217 °C
423 °F
Descriptive Properties Value Comments
FAA Flammability, FAR 25.853 A/B NATURAL
FAR 25.853
NBS Smoke Density, Flaming, Dmax 5
ASTM E 662
NBS Smoke Density, Flaming, Ds 1.5 min 0
ASTM E 662
NBS Smoke Density, Flaming, Ds 4 min 5
ASTM E 662
OSU total heat release (2 minute test) 5kW-min/m^2
FAR 25.853
OSU peak heat release rate (5 minute test) 40kW/m^2
FAR 25.853
Vertical Burn a (60s) passes at 0sec
FAR 25.853
Vertical Burn b (12s) passes at 0sec
FAR 25.853
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved