Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Polymer Resources NY66-M25G15 Nylon 66, 25% Mineral, 15% Glass Reinforced Nylon 66, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gr.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R7543E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ PS-15GF/10T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Polymer Resources NY6-M40 Nylon 6, 40% Mineral Filled Nylon 6, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 80-7705 Polyacetal-copolymer, with carbon fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Suitable for discharging of st.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Greene Tweed Arlon® 1286 Polyketone, Carbon Filled Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including A.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Lord Adhesives Circalokâ„¢ EP-729 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-729 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | ASTM D 792 |
Karina 10/1-FC-LMP White Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Lord Adhesives Circalokâ„¢ EP-939 Epoxy Board Level Encapsulant LORD Thermosetâ„¢ EP-939 encapsulant is a black, one-component epoxy specifically designed to meet the needs of coating semiconductor devices on printed circuit boards.All information provided by.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Sylvin Technologies 9999-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Shin-Etsu Silicones FE-381U Fluorosilicone Elastomer ShinEtsu FE381 U is one of a series of high tensile, high tear fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series fo.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Silberline Aquasil® "BP" SO Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Techmer ES Plaslube® J-1/30/TF/13/SI/2 NAT PA66 |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Samyang Tribit® 1500G10 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G10 is a reinforced, general purpose gr.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gardenia P80515PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80515PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.49 g/cc @Temperature 25.0 °C |
1.49 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® LS 4-9038 FLUOROSILICONE RUBBER 50 Durometer, off-white, uncatalysed, high temperature grade fluorosilicone base.Information provided by Dow Corning |
|||
Specific Gravity | 1.49 g/cc @Temperature 25.0 °C |
1.49 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® LS-2380 FLUOROSILICONE RUBBER 70 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Clariant Renol BR2065 Nylon 66, Mineral/Glass Reinforced Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D-792 |
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4526 CPVC is a pelletized injection molding compound designed for fittings. Typical applications are in potable water and chemical transfer systems especially where high res.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® MFN 6601 Mineral Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gardenia P80515PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80515PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |