Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne LubriOne™ NN-30GF/15T Black Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Nymax™ GMF 600 A 40 Storm Grey Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Ovation Polymers Opnyl LSE - OP66GF3015 Nylon 66 Low surface energy Nylon 66 for demanding applications such as bearings, bushes, rods and gearsAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Edgetek® SF-40CF/000 Polyphenylene Sulfide (PPS) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible D7000 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Greene Tweed Arlon® 1286 Polyketone, Carbon Filled Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including A.. |
|||
Specific Gravity | 1.49 - 1.55 g/cc | 1.49 - 1.55 g/cc | NBR NM-IEC 60811-1-3 |
Karina E 02/5-FC-LMP Yellow Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for electrical wires and cables. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes.Important con.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Sylvin Technologies 9999-75 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D 792 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Silberline Aquasil® "BP" SO Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Shinkong Synthetic Fibers Shinite® D202G15 PBT, 15% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SIG 5001 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: C; D; TI2; YI2; T11; Y11 Agency Ratings: BS 6746; IEC 60227; VDE 0207 Forms: .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gardenia P80515PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80515PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4012 Concentrate Based in Polyethylene DescriptionPOLYBATCH® 4012 is a blur color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 4.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
Trelleborg Hypalon® H608 Chlorosulphonated Polyethylene PropertiesExcellent resistance to oxidation and has outstanding resistance to atmospheric conditions and in particular strong sunlight and ozone.CSM compounds resist fire and are self extinguishing .. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
Aaron Industries AAROPRENE® MFN 6601 Mineral Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Gardenia P80515PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80515PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.49 g/cc | 1.49 g/cc | Method A; ASTM D792 |
LNP Lubricomp® OCL-4536 Polyphenylene Sulfide, Carbon Fiber Reinforced, PTFE + Silicone Lubricant
(discontinu Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |