Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name SABIC PPCOMPOUND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID is 209708556.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D792
Density 0.990 g/cc
0.0358 lb/in³
ISO 1183
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 230 °C
23 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
50 mm/min, 1A; ISO 527
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ISO 527
Elongation at Break 26.7 %
26.7 %
50 mm/min; ISO 527
Elongation at Yield 4.6 %
4.6 %
50 mm/min; ISO 527
Tensile Modulus 1.96 GPa
284 ksi
1 mm/min; ISO 527
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min, 64mm span; ISO 178
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 56.0 µm/m-°C

@Temperature -30.0 - 100 °C
31.1 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
CTE, linear, Transverse to Flow 116 µm/m-°C

@Temperature -30.0 - 100 °C
64.4 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 114 °C
237 °F
80*10*4mm, Cut; ISO 75-1&2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
80*10*4mm, Cut; ISO 75-1&2
Copyright © lookpolymers.com All Rights Reserved