Polymer Property : Dart Drop, Total Energy = 15.5 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® HMG94MD ABS
Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable.
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific)
Superior flow, injection molding ABS. Good impact. For thin-wall applications.
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Cycolac® MG94U ABS
High flow, UV stabilized ABS molding grade
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC
LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing.
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi..
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC
LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare..
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific)
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Dart Drop, Total Energy 21.0 J

@Temperature -15.0 °C
15.5 ft-lb

@Temperature 5.00 °F
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
LyondellBasell Hifaxâ„¢ CB259 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB259 medium high melt flow, 1,600 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact r..
Dart Drop, Total Energy 21.0 J

@Temperature 0.000 °C
15.5 ft-lb

@Temperature 32.0 °F
Peak Energy, 135.0 m/min; ASTM D3763
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of ..
Dart Drop, Total Energy 21.0 J

@Temperature -30.0 °C
15.5 ft-lb

@Temperature -22.0 °F
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi..
Dart Drop, Total Energy 21.0 J

@Temperature -10.0 °C
15.5 ft-lb

@Temperature 14.0 °F
Instrumented, Peak Energy, 405.0 m/min; ASTM D3763
LyondellBasell Hostacomâ„¢ CB280F Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB280F high melt flow, 1,900 MPa flexural modulus, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, ..
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP
SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID..
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific)
LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform..
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11
LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
ASTM Test
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP STAT-KON FX98500C PE
LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE)
LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber.
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.
Dart Drop, Total Energy 21.0 J
15.5 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific)
LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa..
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics NORYL GFN1 PPE+PS
PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui..
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD4412 PC
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East)
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
Dart Drop, Total Energy 21.0 J

@Temperature 23.0 °C
15.5 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific)
Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.