Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 23 g/10 min @Load 3.80 kg, Temperature 230 °C |
23 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 51 HF General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX7259 PC (Asia Pacific) Cycoloy resin grade CX7259 is a flame retardant impact modified polycarbonate blend aiming at ultra thin wall designs. It is listed as UL-94 V1 at 0.5mm & V0 at 0.6mm with excellent flow and balance.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 260 °C |
23 g/10 min @Load 4.76 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 220 °C |
23 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
PTS Trilac® ABS-MP1000 Metal Plating Grade ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVALEN PC 99 GF 30/1M Polypropylene reinforced with glass fiber, improved flowing Modified copolymer PP for injection molding, reinforced with 30% glass fiber, improved flowing. Applied in all industry branches. Delivered in natural mode and in the full RAL color scale.Informatio.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 250 °C |
23 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY GN5001SF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Melt Flow | 23 - 29 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 - 29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 2610 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 23 - 29 g/10 min @Load 2.16 kg, Temperature 235 °C |
23 - 29 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1100-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mitsubishi Iupilon® H2000R 23 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620 PP SABIC® PPcompound 8620 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and good flow with exterior automotive weathering stability. It was origin.. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 250 °C |
23 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® CF-3200HF PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 220 °C |
23 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BF-0670T MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 220 °C |
23 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® AS-0151 ABS, Unreinforced Anti-staticInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang. |
|||
Melt Flow | 23 g/10 min @Load 1.20 kg, Temperature 300 °C |
23 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain.. |
|||
Melt Flow | 23 g/10 min @Load 5.00 kg, Temperature 250 °C |
23 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCD841U PPE-TPE Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE DescriptionPOLYBATCH® FSU-105 is a general-purpose oleamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF va.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE DescriptionPOLYBATCH® FSU-105 is a general-purpose oleamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF va.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ FSU-105 Concentrate Based In LDPE DescriptionPOLYBATCH® FSU-105 is a general-purpose oleamide slip and antiblock concentrate based in LDPE. This material has been designed to offer a 2:1 antiblock slip ratio for films whose COF va.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 160 °C |
23 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1357E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 160 °C |
23 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1365E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 190 °C |
23 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A.. |
|||
Melt Flow | 23 g/10 min | 23 g/10 min | ISO 1133 |
Domo 1040RC Polypropylene Homopolymer Information provided by Domo. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil Exxtral™ MDK340 Performance Polyolefin Product Description: A medium melt flow rate, 40% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc.. |
|||
Melt Flow | 23 g/10 min @Load 2.16 kg, Temperature 230 °C |
23 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Radici Heraflex® E 6521 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Medium-high Modulus, Nominal Shore D/15s 57. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Melt Flow | 23 g/10 min @Load 10.0 kg, Temperature 220 °C |
23 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® SAN C Styrene Acrylonitrile Luran SAN C is an injection molding grade of SAN with medium impact strength and high flow.Information provided by Styrolution |
|||
Melt Flow | 23 g/10 min | 23 g/10 min | ASTM D1238 |
Samyang Trilen® 9550T30 Polypropylene, Reinforced Mechanical strength and thermal resistance are excellent.9550T30 is a non-flame retardant, reinforced grade.Information provided by Samyang. |