Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Noryl GTX GTX6013 PPE+PA6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl GTX GTX6013 PPE+PA6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D 792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm

@Thickness 3.20 mm
0.0070 - 0.0090 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
SABIC - Japan Method
Elongation at Break 180 %
180 %
SABIC - Japan Method
Flexural Strength 93.0 MPa
13500 psi
ASTM D 790
Flexural Modulus 2.25 GPa
326 ksi
ASTM D 790
Izod Impact, Notched 6.08 J/cm

@Temperature 23.0 °C
11.4 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
CTE, linear 75.0 - 85.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
41.7 - 47.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 190 °C

@Thickness 3.20 mm
374 °F

@Thickness 0.126 in
unannealed; ASTM D 648