Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.10 J/cm | 11.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 6.10 J/cm | 11.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 6.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
11.4 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA426 Black 2880 Polyvinyl Chloride Alloy (PVC Alloy) Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426 Black 2880.Information provided by PolyOne |
|||
Izod Impact, Notched | 6.10 J/cm | 11.4 ft-lb/in | ASTM D256 |
Global PC/ABS QX-7004 Molding Grade PC/ABS
(discontinued **) Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 6.10 J/cm | 11.4 ft-lb/in | ASTM D256 |
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Izod Impact, Notched | 6.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.4 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PC-S923 Modified PC Features:Excellent balance propertiesGood weather resistanceHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElec.. |
|||
Izod Impact, Notched | >= 6.08 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 11.4 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Izod Impact, Notched | 6.10 J/cm | 11.4 ft-lb/in | edgewise; ASTM D256 |
Haysite EHC Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) This IEEE Class F 155ºC high strength material exhibits substantial resistance to cold flow or creep under heat and pressure. Suggested applications include motor slot wedges, washers, brush plat.. |
|||
Izod Impact, Notched | 6.06 J/cm | 11.4 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354 PC+ABS (Asia Pacific) This is a PC/ABS compound, a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 6.08 J/cm @Temperature 23.0 °C |
11.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX6013 PPE+PA6 (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.10 J/cm | 11.4 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® G70FR , Flame Retardant, Un-Reinforced PC/ABS Alloy Flame Retardant, Impact ResistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 6.10 J/cm @Temperature -30.0 °C |
11.4 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML1661 PC Copolymer (Asia Pacific) Medium-flow impact-modified light-shielding high-flow-ductile PC copolymer. Available in white color only. |